Chromium Metal Low Nitrogen Grade SD50 & SD25
Chromium metal is manufactured by the aluminothermic reduction of chromium oxide and is crushed and ground to specific size requirements.
The special degassed (SD) low nitrogen chromium metal developed by LSM is used for applications in the production of superalloys, which are used to improve heat, wear and corrosion resistance.
Download our product sheet for more details.
Various compositions are available upon request.
Please contact us to discuss your requirements.
Size
Available in lump or granular form to requirements.
Packaging
Uniform nett weight steel drums or as specified.